We visited a large commercial bakery in April where the case erecting line, a Bedo case erector running off a Nordson ProBlue 4 tank, packing shipper cases of croissants, had exactly that reputation. Stringing had been an issue on the line for as long as anyone could remember. It was accepted as the price of running the machine.
It isn't. Stringing is a symptom, and it's fixable.
- Field Report
- Bakery
- Case Erection
- Bedo
- Nordson ProBlue
- Stringing & Tailing
- UltimateCool
What stringing actually is
When a hot melt nozzle fires and cuts off, the adhesive should snap cleanly. If the glue is too stringy at its running temperature, or it's being run too hot or too cold for its formulation, it draws out a fine tail instead. That tail lands somewhere it shouldn't: the machine, the guarding, the next box, the floor.
One string is nothing. Thousands of them per shift become fouled sensors, glue on packaging that reaches your customer, cleaning time you shouldn't need, and adhesive you paid for decorating your machinery instead of holding boxes shut.
What we found on this line
The incumbent adhesive was running at 140°C in the tank, 150°C in the hoses and 160°C at the guns, and the line was stringing heavily. Bond quality was patchy too. Boxes showed strong fibre tear on one flap and almost none on the other.
We drained the system down and swapped it over to UltimateCool 98 Plus with a colour trace so we could see exactly when the new adhesive was through the system. Then we dropped the temperatures to 115°C in the tank and 120°C in the hoses and guns.



The stringing stopped. The bonds gave excellent fibre tear. And when we ran a taped up case through to measure how much adhesive the line was actually applying, the numbers surprised even us: 5.85 grams per case on the old adhesive, 3.60 grams on the new one. That's around 38% less glue doing a better job, at temperatures 40°C cooler.
The honest caveats
We always report what we see, including the awkward bits. On this trial one hose was partially blocked, which means the exact 38% figure should be treated with a little caution until it's verified over a longer run. The direction of travel is not in doubt though: cleaner cut off, stronger bonds and a meaningful drop in consumption.
That's the point of a trial. One day on your line, measured in the open, before you commit to anything.
If your line has "always done that"
Stringing, tailing, patchy bonds, glue everywhere: none of these are personality traits of your machine. They are usually the wrong adhesive, the wrong temperature, or both. We've written a whole whitepaper on stringing if you want the detail, or we can simply come and look at your line.
Small print: Figures from a genuine Alphabond trial carried out in April 2026. Customer details withheld at our discretion.