Alphabond Field Report
Same Tray. Half the Glue. How Much Adhesive Is Your Line Wasting?
Here's a question most packaging managers can't answer: how many grams of adhesive does your line put on each case or tray?
Almost nobody knows, because almost nobody weighs it. Adhesive gets bought by the pallet, tipped into the tank and forgotten about until the next order. Which is a shame, because the gap between what a line applies and what a bond actually needs is often enormous, and it's pure cost.
- Field Report
- Wholesale & Distribution
- Tray Erection
- Lantech
- Robatech Concept
- Consumption Saving
- Perfecta
- UltimateCool
How you measure it
The method is beautifully simple. Tape up a tray so the glue can't bond to it, send it down the line as normal, then peel the adhesive off and weigh it. That's your true applied weight per tray, not a datasheet estimate.
We did exactly this at a national wholesale distributor in June, on a Lantech tray former coupled to a Robatech Concept tank with an autofeeder, erecting the corrugate trays their warehouse ships in. The incumbent adhesive weighed in at 3.02 grams per tray.
Round one: a like for like swap
First we switched the tank to Perfecta 3, our workhorse packaging grade, and dropped the hose and gun temperatures slightly. Fibre tear stayed excellent, meaning the cardboard rips before the bond lets go, and the taped tray came back at 2.45 grams.
Same tray, same speed, same strong bond. 19% less glue.
Round two: turning the temperature right down
Then we went further and ran UltimateCool 98, a low temperature grade, taking the tank from 150°C down to 101°C. After a small pressure adjustment the bonds were strong with excellent fibre tear, and the weighed tray came back at 1.56 grams.




That's a 48% reduction against the original adhesive. We'd be the first to say that figure needs validating over a longer run, since a little of the old higher temperature adhesive may still have been in the system. Call it "up to 48%" and verify it on an extended trial. Even the cautious reading is a consumption saving of a fifth to a third, plus everything that comes with running a tank 50 degrees cooler: less energy, less char, fewer blocked nozzles and a safer machine to work around.
Why less glue means better bonds
It sounds backwards, but over application is one of the most common faults we find on trials. Too much hot melt slows the set, invites stringing, squeezes out of the joint and wastes money on every single case. A modern adhesive with higher bond strength does more with less. The weighing exercise just makes the difference impossible to argue with.
Get your line weighed
The whole trial took a morning, and the customer watched every measurement happen on their own line. If you'd like the same numbers for your line, we'll come and get them for you, free, and you keep the report either way.
Small print: Figures from a genuine Alphabond trial carried out in June 2026. Customer details withheld at our discretion.
Want the same numbers for your line?
One day on your line, with your product and your team watching. We bring the kit, do the maths and leave you the report either way.
Book a free trial on your line