Alphabond Field Report

    Nobody Had The Password To Their Own Tank

    Half the time a hot melt tank is running hotter than it needs to, it isn't really a decision anyone made. It's just a setting nobody has touched, and on this trial, nobody could touch it even if they'd wanted to.

    We were on site to trial UltimateCool 98 Plus, a low temperature grade, on a case erector running outer cases on a bottling line. The incumbent adhesive was set at 150°C in the tank, 155°C in the hose and 160°C at the gun, numbers that had presumably been fine once and never revisited.

    • Field Report
    • Beverage
    • Case Erection
    • Energy Saving
    • Consumption Saving
    • UltimateCool

    An adhesive nobody could get to

    The tank arrived unmolten, adding some time before the trial could even start. Once it had melted through and drained low enough, we got a baseline coat weight on a taped-up case: 1.93 grams.

    We then topped up with UltimateCool 98 Plus, purged through with a colour drop to confirm the new adhesive was running clean, and went to lower the temperature. That's where it stalled. The tank's temperature controls were password protected, and nobody on site had the password.

    It took a while to track it down and get in. Once we did, we set the tank to 105°C, the hose to 115°C and the gun to 120°C, a drop of up to 55°C from where the incumbent had been running.

    Hot melt tank with unmolten adhesive pellets floating on the surfaceTank drained low before topping up with the trial adhesiveUltimateCool 98 Plus purging through with a colour drop to confirm the changeoverScales showing 1.93 grams of adhesive from the incumbent productScales showing 1.01 grams of adhesive with UltimateCool 98 Plus

    What the numbers said

    With the tank cooling from 160°C down to 105°C, there was a natural pause while temperatures settled, so we broke for lunch and came back to finish the trial. Once the line was back up at the new settings, bonds were strong with full fibre tear.

    A taped-up case sent through gave a new coat weight of 1.01 grams. That's a 48% cut in adhesive use, on the same cases, at the same line speed, from the same operators, without weakening a single bond.

    Why the password mattered as much as the adhesive

    A locked control panel isn't a footnote here, it's the whole story. Plenty of lines run hot not because anyone chose it, but because whoever set it up years ago is long gone and the settings became untouchable by accident. The trial only worked once that barrier was cleared. Worth asking on your own line: does anyone still have the password?

    What's next

    This was a single visit, so the next step recommended is a pallet-quantity extended trial to confirm the longer term benefits, including energy use and nozzle blockages, over a full production run.

    Small print: Figures from a genuine Alphabond trial. Customer details withheld at our discretion.

    Want the same numbers for your line?

    One day on your line, with your product and your team watching. We bring the kit, do the maths and leave you the report either way.

    Book a free trial on your line